Keeping the shine

Toyotech

New Member
Since The Norton is in pieces to start, I decided to detail all the bits & pieces as I assemble in order to do it right the first time. I polished the engine timing cover, gear box cover, primary cover & lower fork bodies this last week while it's been slow at work (I really raised the bar for myself this time). I read in another thread about VHT high temp clear coating and will be using that on the polished aluminum bits so I don't have to break out the Mother's every other day to keep it gleaming.

What is the best way to prep the parts for coating without losing any of the luster and still have a proper surface for the VHT to adhere? Also, if I use VHT black on the cylinder jugs, do I need to cure it twice or just after I clear over the black? When I cure it in the oven at 200 degrees F for 20 minutes, am I at risk of warping the jugs?

Any input on any of these concerns would be greatly appreciated!

Cheers!
 
I've never had any luck getting paint (clear or otherwise) to stick to polished aluminum.
That being said, I think your best bet is to wipe it with a solvent that'll flash off and paint it immediately.

200* shouldn't warp your cylinders, they're regularly abused with higher temps....
 
You want to keep a shiny polished aluminum surface on your parts by painting them clear?

Its going to run like a 100 meter sprint if you try that. If you try light dusty/ dry over spray coats, it wont be shiny. The paint needs something to cure in to. If you do some how manage to get the paint on there then wet sand it without going through your clear to the metal, expect your paint to flake off.

May I suggest some kind of wax? Ive never tried that one before but if it seals the metal from the O2 in the air, I don't see why it wouldn't keep a nice shine.
 
Toyotech, Excellent bike of choice :o. Not sure what VHT is but I think it's not rattle can clear. Hope someone has knowledge of this as I'm curious too.
 
That's kind of the answers that I was expecting. Oh, well, I guess I'll be buying Mother's by the gallon! As far as the cylinder jugs are concerned, I was thinking as long as it cools evenly, I think it should be all right. Thanks, guys
 
there is no need to cure the paint in the oven for engine parts because itll get up to the 200* after its assembled and running, unless your afraid of being clumsy and spilling gas or something on it before it gets to run.
 
forcefanajd said:
there is no need to cure the paint in the oven for engine parts because itll get up to the 200* after its assembled and running, unless your afraid of being clumsy and spilling gas or something on it before it gets to run.

Thanks, that sounds like a plan. Question is now, how soon after assembly do I have to have it running for proper curing? It could be as long as a couple of months from the time I paint and actually have a running engine. As far as spilling gas, I can be quite careful when the need arises!
 
There should be detailed directions on the back of the can. But basically the paint will be fine without the "high heat curing" if all you're doing is touching it, reassembly, etc. Whenever it cures it will become more resistant to gas, oil, cleaners, and the like. Can't imagine why a couple months sitting around first would hurt it.

And for the record - VHT states to cure the part at certain temps for certain amounts of time with cool off periods between. But NEVER exceed the max operating temp of the part in question.
 
Were it me, I'd go ahead and bake it in an oven anyway. The cylinder will heat unevenly, being much hotter closer to the sleeve and that paint may well burn away rather than curing to a hard consistency. If you bake it in an oven the heat will be consistent and can be controlled much easier.

just a thought
 
Try Turtle Wax Ice. Its a liquid polish that Ive heard great things about. Not sure about on motor parts (bc of heat) but it should say on the bottle.
 
Back
Top Bottom