So I started electrolysis this weekend. I tried my luck last week but I bought a charger that was "too smart" for this job. went back and paid a little more money, but I hope in the end it'll be worth it. Before I started electrolysis, I used the product Metal Rescue for a few days. I want to say that that did a number on the tank to start because of the black liquid (that was once clear) that poured out of the tank when I finished.

here is the set up:

69e0e622.jpg


I used Distilled Water b/c it's the cleanest thing I could get:

22c695ba.jpg


With Washing Soda, which, incase you didn't know, is really fucking hard to find and I ended up having to go to the dreaded WalMart as a last resort to buy it (grrrrrrr):

a3e1ef7c.jpg


I plugged up the bung with a rubber stopper:

4f252767.jpg


and this is the trickle charger I am using on 2amps:

64f55dd7.jpg


I used 8tsp to a gallon of the Washing Soda. There is about 2 cups of soda in there (8tsp = 1/2 cup). At the beginning, I was working pretty well however, now Im not getting much of a response out of the set up. It might be that I got most of the rust out with the metal rescue, but the spine of the tank is still in really rough shape.

b792a3b0.jpg


I can hear the bubbles working. idk. Maybe that part of the tank is just gone and I have to por 15 over it.
 
When I did my tank it worked fine. I just didnt clean it out properlly. I would just say get a POR 15 kit, Kreem kit, if money is not tight. seals it up also.
 
I already have the Por 15 kit. Im doing this before the sealer. The tank is in bad on the inside.
 
sxecafe said:
I already have the Por 15 kit. Im doing this before the sealer. The tank is in bad on the inside.
Oh, I did practically the same thing, just stronger charger and a bigger positive ground. I lefted mine for about 12 hours. Some people leave it for 24 hours.
 
what was your charge charge and what do you mean bigger positive ground?
 
I seriously thought for a minute that someone was posting about hair removal on a motorcycle site. Thank God it turned out I was wrong. Freaking 'electrolysis.'
 
I think I had it at 12v 40 amps now that I think about it. But I left it on with 12v 200amps for awhile. And I mean the metal the positive cable goes on that attracts the rust.
 
sxecafe said:
I already have the Por 15 kit. Im doing this before the sealer. The tank is in bad on the inside.

If you have the POR-15 KIT, you don't have to do any of this. It comes with the cleaners and etchers that will completely clean your tank to bare, raw metal. Doing the electrolysis before hand is just wasted effort.

I just did a tank yesterday with POR-15. The tank was coated with varnish and rust inside, with loose flakes of rust everywhere. The only pre-prep I did was to vacuum out the loose rust, shake some drywall screws around inside, and vacuum again. The POR Marine Clean and Metal Etch/Prep made the interior absolutely pristine before doing the coating.
 
I have used POr before and this tank seems pretty shotty on the inside. I have watched a few people prep really rusted tanks by doing this first, so I dont think it would hurt. I dont know if the Marine clean and Etch/Prep will take the thing to bare metal but, tonight I drained out the tank and I'm going to use the Por prep this week so we shall see.
 
Is there a particular type of anode that works better than others (ie - different metals)?
 
What did your electrode look like? The reaction happens line-of-sight mostly, so if you move the electrode around and maybe orient it parallel with the tunnel, you might get better results. Also, I'd crank the amps up, 2A is barely enough.

Just curious, is there an escape path for the hydrogen? I don't think it will effect the chemistry but it might pop the cork.
 
I had the electrode in various places in the tank. The first was like a tuning fork but it went beyond the spine of the tank. The I did a single "finger" down either side and lastly I tried to have a different, shorter wire to get just the spine. I ran the cycle on 10a for a while as well.

And yes, its just a rattle can cap so there is that little hole on the side that can help you pop the cap off the can, if that makes sense. I could hear the bubbles working, if that's any indication.
 
sxecafe said:

That looks like paint or some sort of coating in there. Are you sure the tank hasn't been coated before? If it has, you'll need to get rid of the coating for the electrolosis to work properly.
 
I have no idea. How would I be able to tell? Even more important, how would I get rid of it?
 
I 've bee after the misses,,too yous some electroisis.......cause shes got a bad moustash,,,,,hairs on the upper lips,,,,aints wright...........good luck with your gas tank
 
Hills I think you're right. I came home and took a small chisel and lightly touched the spine and it came up.

4f721b07.jpg


I guess now the question is how to get that up. Would the marine clean that they give you work?
 